Persona di contatto : Murphy
Numero di telefono : +86 18990025049
whatsapp : +8618990025049

SF-3M AlTiN Coated Diamond Cut Carbide Burr for Stainless Steel and Superalloys

Luogo di origine Cina
Marca CABURTECH
Certificazione ISO9001:2008
Numero di modello SF-3MDM
Quantità di ordine minimo 50 pz
Prezzo 1-5usd/pc
Imballaggi particolari cartone43*25*22,5 cm
Tempi di consegna 15-30 giorni
Termini di pagamento T/T,L/C,Western Union
Capacità di alimentazione 70000pcs/month
Dettagli
Modello SF-3MDM Taglia Dia 9,6 mm
Tagliare la lunghezza 19 mm Gambo dia 6 mm
In generale 64 mm Materiale Carburo di tungsteno
Grado Yg8 Taglio Taglio del diamante
Tipo Brasatura d'argento Pezzo in lavorazione Ghisa d'acciaio e
Rivestimento Altin
Evidenziare

AlTiN Coated Carbide Burr

,

Diamond Cut Rotary Burr

,

Tungsten Carbide Diamond Cut Burr

Lasciate un messaggio
Descrizione di prodotto

SF-3M AlTiN Coated Diamond Cut Burr – For Stainless Steel and Superalloys


The SF-3M is a diamond cut carbide burr with an AlTiN coating. Diamond cut means the teeth are arranged in a cross pattern, which helps break chips into small pieces. This makes it easier to cut tough materials like stainless steel and superalloys without the chips tangling around the tool. The AlTiN coating adds heat resistance and helps the burr stay sharp longer.


Technical Parameters
Model Cut dia (D1) Cut length (D2) Shank (L1) Overall (L2) Type Cut
SF-3M DM 9.6 19 6 64 Silver braz Diamond



This burr is a good choice for weld removal, deburring, and surface blending on hard metals. The combination of diamond cut and AlTiN coating means it cuts efficiently while resisting wear and heat buildup. It works with standard die grinders and is reliable for daily use in tool shops and industrial maintenance.


SF-3M AlTiN Coated Diamond Cut Carbide Burr for Stainless Steel and Superalloys 0


Caburtech offers a wide selection of carbide burr shapes in Single and Double Cut styles, including Cylinder, Round nose cylinder, Ball, Oval, Tree, Flame, Cone, Countersink and Inverted Cone. Each shape is designed for grinding, deburring, chamfering, and finishing on steels under 60 HRC, stainless steels, cast iron and etc.

 

FAQ

1.How to Use:

This product belongs to the commonly used alloy consumables, and is designed to be used with high-speed electric grinders or pneumatic tools.

2.OEM:

We offer OEM services to cater to specific customer requirements.

3.MOQ:

The usual minimum order quantity is 100 pcs per model.

However, this can be adjusted based on your specific requirements. Please consult your sales representative for further details.

4.Lead Time:

The lead time for regular orders is approximately one month, excluding samples.

5.Port:

Shanghai/ Guangzhou/ Shenzhen/ Ningbo/ Yiwu/ Chengdu.